Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Feature: | Transparent |
| CAS No.: | 9003-56-9 |
Suppliers with verified business licenses

Physical Properties | Test Conditions | Test Methods | Test Results | Units |
Density | 23°C | ISO1183 | 1.08 | g/cm³ |
Melt Mass - Flow Rate | 200°C/5.0kg | ASTMD1238,ISO1133 | 3 | g/10min |
Shrinkage | ISO294-4 | 0.30-0.70 | % | |
Density | -- | ASTMD792 | 1.08 | g/cm³ |
Mechanical Properties | Test Conditions | Test Methods | Test Results | Units |
Elongation | break3 | ASTMD638 | 40 | % |
break | ISO527-2/50 | 40 | % | |
Flexural Modulus | --4 | ASTMD790 | 1900 | Mpa |
--5 | ISO178 | 1900 | Mpa | |
Tensile Strength | yiled | ISO527-2/50 | 42 | Mpa |
Izod Notched Impact Strength | 23°C | ISO180/1A | 14 | kJ/m² |
Flexural Strength | --4 | ASTMD790 | 53.9 | Mpa |
--5 | ISO178 | 57 | Mpa | |
Charpy Notched Impact Strength | -30°C | ISO179 | 7 | kJ/m² |
23°C | ISO179 | 14 | kJ/m² | |
Izod Notched Impact Strength | 23°C,3.20mm | ASTMD256 | 150 | J/m |
23°C,6.40mm | ASTMD256 | 160 | J/m | |
-30°C | ISO180/1A | 7 | kJ/m² | |
Tensile Strength | break | ISO527-2/50 | 33 | Mpa |
--3 | ASTMD638 | 39.7 | Mpa | |
Thermal Properties | Test Conditions | Test Methods | Test Results | Units |
Heat Deflection Temperature | 1.8MPa,Unannealed | ASTMD648 | 88 | °C |
1.8MPa,Unannealed | ISO75-2/A | 77 | °C | |
1.8MPa,annealed | ASTMD648 | 99 | °C | |
1.8MPa,annealed | ISO75-2/A | 97 | °C | |
Vicat Softening Point | -- | ASTMD15256 | 105 | °C |
-- | ISO306/A50 | 104 | °C | |
-- | ISO306/B50 | 96 | °C | |
Linear Thermal Expansion Coefficient | MD | ISO11359-2 | 9.00E-05 | cm/cm/°C |